| BEFORE
These two-iron parts were produced using the
sand-casting process. Several secondary machining
operations were required to properly fit carbide
drilling inserts into the internal detail
of the parts. Notice the rough finish and
lack of detail. |
AFTER
We reduced the machining operation cost for
these two parts by using the investment casting
process. These parts were cast to net shape,
eliminating all machining operations. Cast
from high strength steel alloy, these parts
now have superior detail - see the detail
in the part number. |